Typical Properties
Melt Flow Rate (190 °C/2.16 kg)
0.20 g/10 min
Density (23 °C)
0.946 g/cm³
Flexural Modulus (1% Secant)
140000 psi
Tensile Strength at Yield
3400 psi
Tensile Elongation at Break
>800 %
Environmental Stress Crack Resistance F₅₀ (100% Igepal®, Cond B)
>1000 hr
Tensile Impact Strength
245 ft-lb/in²
Shore Hardness (Shore D)
65
Vicat Softening Temperature
122 °C
Low Temperature Brittleness F₅₀
<-76 °C
Deflection Temperature Under Load (66 psi, Unannealed)
66 °C
Antistat
None ppm